Figure 2.

Figure 2

TGA curves of analyzed blend samples filled with MA treated cellulose fibers (regular chemical modification approach) dried either not dried before the carried out process; UFC100/D/1440—cellulose fibers dried for 1440 min (24 h) at 100 °C.