Evolution of the sheet resistance of the washed electrodes from different sublots (S1, S2, S3, S4).

S1 S2 S3 S4
Yarn A B C A B C A B C A B C
R10/R0 1.30 1.43 1.25 0.87 0.84 1.03 0.96 0.84 0.90 1.25 1.51 2.01
R20/R0 1.33 1.88 1.24 0.92 1.05 0.92 0.82 0.83 0.76 1.50 1.47 2.81
R30/R0 1.47 1.61 1.47 0.88 0.90 0.83 0.91 1.10 0.89 1.13 1.37 3.86