Printing parameters for obtaining Polycaprolactone (PCL) and PCL/Thermally Reduced Graphene Oxide (TrGO) scaffolds.

MATERIAL PCL TRGO
Temperature 170 °C 220 °C
Atmosphere Nitrogen Nitrogen
Pressure 4.5 bar 6 bar
Robot Head Velocity 0.5 mm/s 0.3 mm/s
Pre-flow 2 s 2.5 s
Post-flow 1.5 s 2 s
Needle inner Diameter 0.9 mm-20 g 0.9 mm-20 g
Warm up Time 50 min 60 min