Skip to main content
. 2020 Apr 12;2020:4783612. doi: 10.1155/2020/4783612

Figure 11.

Figure 11

Particle size analysis. (a) Fe3O4 NPs synthesized using the Tween-80 surfactant at 30°C. (b) Silica-coated Fe3O4 NPs synthesized using the Tween-80 surfactant at 30°C. (c) Fe3O4 NPs synthesized using SDS surfactant at 30°C. (d) SEM micrographs of Fe3O4 synthesized using the Tween-80 surfactant after the DLS analysis.