Skip to main content
. 2020 Apr 5;10(2):128–134. doi: 10.1016/j.jobcr.2020.03.008

Table 2.

Comparison of shear bond strength between the control and Cinnamon powder modified resin.

Study group Mean SD T value P value
Control 8.50 1.66 1.22 0.256
Experimental 7.20 1.68