TABLE 2.

BET surface area (m2/g) of wood of transgenic and wild-type (WT) hybrid aspen with and without acid pretreatment.a,b

Wood samples Non-pretreated wood Acid-pretreated wood
11 2.06 ± 0.04*** 3.22 ± 0.09
14B 1.91 ± 0.13* 3.29 ± 0.26*
14C 1.75 ± 0.07 3.33 ± 0.08**
Trans 1.91 ± 0.15*** 3.28 ± 0.15**
WT 1.72 ± 0.07 2.96 ± 0.02

aAnalyses were based on samples consisting of pooled wood from four separate trees. Each sample was analyzed as technical triplicates. bStatistical significance is based on ANOVA with post hoc Dunnett test for each transgenic line and on contrast for all transgenic lines (Trans) together: ∗∗∗P ≤ 0.01; ∗∗P ≤ 0.05; P ≤ 0.1.