Figure 1

Size distribution of the PS emulsions. (A) PS emulsion produced by LCTs, with the WPI (0.5%, w/w)-T80 (1.5%, w/w) as the emulsifier; (B) PS emulsion produced by MCTs, with T80 (2.0%, w/w) as the emulsifier.