Table 3.
polymer | pKa1 | pKa2 | macroscopic behavior |
---|---|---|---|
SMA-Glu | 7.4 | no precipitated observed | |
SMA-Neut | 6.4 | 10.4 | no precipitated observed |
SMA-AE | 9.5 | above pH 2.3, the undissolved material swells and forms a gel-like phase. Below pH 2.3, the transparent solution becomes cloudy, and the nebulous material settles to bottom within 24 h. | |