Skip to main content
. 2020 Apr 15;8:213. doi: 10.3389/fchem.2020.00213

Figure 5.

Figure 5

The images from SEM analysis showed the surface (A: SL, B: SLC, C: SLE, D: SLEC) and cross sections (E: SL, F: SLC, G: SLE, H: SLEC). The cross sections showed that nanocellulose reinforcement into PLA (F,H) have smaller pores compared to without nanocellulose (E,G) (adapted, with permission from Yu et al., 2019).