Table 4.

Results of internal fit measurement (pooled data for the three evaluation methods, COM = resin composite, ZIR = zirconium dioxide and NPA = non-precious alloy).

Measurement Position Internal Gap
(mean (SD) [µm])
Internal Gap – Cement Space = Absolute Discrepancy (Mean (SD) [µm])
COM ZIR NPA COM ZIR NPA
marginal fit (n = 120) 76.4 (0.5) 78.1 (0.5) 80.1 (0.6) −3.6 (0.5) −1.9 (0.5) 0.1 (0.6)
axial fit (n = 120) 97.8 (0.6) 101.8 (0.5) 114.3 (1.1) 17.8 (0.6) 21.8 (0.5) 34.3 (1.1)
occlusal fit (n = 240) 208.5 (1.5) 277.6 (2.2) 455.0 (5.5) 128.5 (1.5) 197.6 (2.2) 375.0 (5.5)