Skip to main content
. 2020 Apr 1;13(7):1610. doi: 10.3390/ma13071610

Figure 5.

Figure 5

Evolution of Vickers hardness from the bottom (first layer) to the top of the wall, for three different material conditions (as-built, T6 and T73).