Skip to main content
. 2020 Apr 3;13(7):1678. doi: 10.3390/ma13071678

Figure 10.

Figure 10

SEM images of the fractured surfaces of PLA specimens. (a) Upright. (b) Flat. (c) Curved. (d) Curved CFFRP.