. 2020 Apr 8;13(7):1739. doi: 10.3390/ma13071739

Table 1.

Shear strength and crystallinity of the SRC obtained at different temperatures and pressures.

Hot Compaction Temperature, °C 25 MPa 50 MPa
Shear Strength, MPa Crystallinity, % Shear Strength, MPa Crystallinity, %
155 2.10 ± 0.10 92.0 ± 1.1 1.10 ± 0.12 94.0 ± 0.9
160 2.20 ± 0.11 91.0 ± 1.3 1.40 ± 0.16 93.0 ± 1.2
165 2.90 ± 0.12 87.0 ± 0.9 2.30 ± 0.18 89.0 ± 1.3
170 3.80 ± 0.14 69.0 ± 1.2 2.90 ± 0.09 84.0 ± 1.7