Table 1.
Type of Powder | Powder Treatment | Fibers Used | Fabrication of Samples | Post-Treatment of Samples |
---|---|---|---|---|
Irregular SiC (d50 = 38.3 µm) | None (1) Milling; (2) Mixing with 5 wt.% of Si powder; (3) Spray drying; (4) Plasma treatment |
30% vol. of SiC fibers mixed with the SiC powder | Binder jetting | SMP-10 infiltration and pyrolysis |