Table 1. Electrospinning Conditions Applied for the Fabrication of Nanofibrous PCL.
| PCL | |
| distance between electrodes [mm] | 180 |
| high voltage [kV] | –10/+40 |
| rewinding speed [mm/min] | 40 |
| steel orifice diameter [mm] | 0.6 |
| temperature [°C] | 22 |
| relative humidity [%] | 50 |