Table 1. Electrospinning Conditions Applied for the Fabrication of Nanofibrous PCL.
PCL | |
distance between electrodes [mm] | 180 |
high voltage [kV] | –10/+40 |
rewinding speed [mm/min] | 40 |
steel orifice diameter [mm] | 0.6 |
temperature [°C] | 22 |
relative humidity [%] | 50 |