Figure 2.

Figure 2

(a) Seed 1h, annealing 180 °C 1 h, CBD 30 min; (b) Seed 1 h, annealing 180 °C 1 h, CBD 1 h (scale bar 1 μm); (c) SEM high magnification image of ZnO nanorods (scale bar 200 nm).