Skip to main content
. 2020 Mar 30;120(8):3890–3938. doi: 10.1021/acs.chemrev.9b00662

Figure 3.

Figure 3

HAADF-STEM images of Au catalysts samples after reduction at 200 °C for 2 h in flowing hydrogen supported by (a) MCM-41, (b) SBA-15 with 4.8 nm thick pore walls, (c) SBA-15 with 2.6 nm-thick pore walls, (d) HMM-2, (e) SBA-12, and (f) SBA-11. Reproduced with permission from ref (75). Copyright 2005 American Chemical Society.