Skip to main content
. 2020 Mar 3;12(3):559. doi: 10.3390/polym12030559

Figure 4.

Figure 4

Raman spectroscopy of all films in this study, (a) denotes the EMI:TFSI treated films from 0% to 2.5% concentrations, meanwhile (b) corresponds to the NaBH4-DMSO solution treatment on the 0% to 2.5% EMIM:TFSI films.