Skip to main content
. 2020 Mar 23;12(3):713. doi: 10.3390/polym12030713

Figure 5.

Figure 5

The comparison of the relative resistance change vs. the deformation for the MWCNTs (pure) (A) and MWCNTs (KMnO4) (B) sensor in six extension/relaxation cycles induced by the tensile stress (from 0.167 to 1.066 MPa). The tensile stresses are the same for both measurements. The deformation is denoted by red circles, the relative resistance changes by black circles.