Table 1.

Characteristics of hydrogel-based optical fibres and waveguides reported in the literature.

Ref. Material Type Dimensions Optical loss
This Agarose Structured fibre 0.64 mm core, 2.5 mm cladding (diameter) 3.23 dB/cm(633 nm)
4 Agarose Rib waveguide 130 × 130 µm² (cross-section area) 13 dB/cm(633 nm)
23 Gelatin core, agarose cladding Planar waveguide 2 µm–2 mm core (thickness) N/A
7 Polyethylene glycol diacrylate (PEGDA) Planar waveguide 1 × 4 mm² (cross-section area) 0.17–0.68 dB/cm(450–550 nm)
18 PEGDA Planar waveguide 1.1 ×5 mm² (cross-section area) 1.7–2.8 dB/cm(450–750 nm)
1 PEGDA core, alginate cladding Fibre 0.2–1 mm core, 0.4–1.2 mm cladding (diameter) 0.3 dB/cm(492 nm)
6 PEGDA core, alginate cladding Fibre 0.2–2 mm core, 0.3–2.2 mm cladding (diameter) 2.6–8.3 dB/cm(532 nm)
19 PEGDA core, alginate cladding Fibre 0.2–2 mm core, 0.3–2.2 mm cladding 1–6 dB/cm(532 nm)
20 Alginate-polyacrylamide Fibre 0.4–1.1 mm core, 0.9–2.2 mm cladding 0.45 dB/cm(532 nm)