Glass transition temperature of silver-containing nanocomposites.

The polymeric systems obtained by using various reducing agent Тg, Тf,
°С °С
Pectin 60
IPEC 53 319
IPEC–Ag (NaBH4) 50 323
IPEC–Ag (N2H4) 82 335
IPEC–Ag (C6H8O6) 61 210