Skip to main content
. 2020 Apr 19;13(8):1930. doi: 10.3390/ma13081930

Figure 4.

Figure 4

The distribution of microhardness in the investigated composite in the as-welded state (EXW) and after hot-rolling (300C, 350C, 400C).