Skip to main content
. 2020 Apr 19;13(8):1930. doi: 10.3390/ma13081930

Figure 8.

Figure 8

The results of the element distribution on the fracture surface of Mg/Al mini-specimen after hot-rolling at 400 °C: aluminum (A) and magnesium (B).