Skip to main content
. 2020 Apr 19;13(8):1930. doi: 10.3390/ma13081930

Figure 18.

Figure 18

TEM image of AA1050/Ti6Al4V joint microstructure in hot-rolled state (A), with selected area diffraction patterns (SAED) (B). TEM lamella position in Figure 17.