The designation of the samples.

Designation State of the Sample
EXW Mg/Al/Ti composite in the as-welded state
300C Mg/Al/Ti composite subjected to the post-weld hot-rolling at 300 °C
350C Mg/Al/Ti composite subjected to the post-weld hot-rolling at 350 °C
400C Mg/Al/Ti composite subjected to the post-weld hot-rolling at 400 °C