Table 1.
Starch | Self-assembly conditions | References |
---|---|---|
Waxy rice | Pullulanase hydrolysis at 58 °C for 8 h and discarding precipitate, followed by self-assembly at 4 °C for 8 h, annealing at 55 °C for 6, 12, 24, and 48 h | Ji et al. (2019) |
Waxy maize |
Pullulanase hydrolysis at 58 °C for 8 h and discarding precipitate, then addition of 0.1% of surfactant (SDS, Span 80 and Tween 80) based on solution, followed by self-assembly at 4 °C for 8 h Isoamylase hydrolysis at 40 °C for 24 and 48 h and discarding precipitate, followed by self-assembly at 4, 25 and 50 °C for 96 h Pullulanase hydrolysis at 58 °C for 8 h and discarding precipitate, followed by self-assembly at 4 °C for 8 h Isoamylase hydrolysis at 50 °C for 24 h and discarding precipitate, followed by self-assembly at 4, 25 and 50 °C for 24 h Pullulanase hydrolysis at 60 °C for 24 h and discarding precipitate, followed by self-assembly at 4 °C for 24 h Pullulanase hydrolysis at 37 °C for 24 h and discarding precipitate, and addition of chitosan to a final concentration of 0.05%, followed by self-assembly at 4 °C for 24 h |
Li et al. (2016) Lee et al. (2019) Jiang et al. (2016b) Jiang et al. (2018) Ji et al. (2015) Cai and Shi (2014) Luo et al. (2019b) Luo et al. (2019a) |
Waxy potato | Isoamylase hydrolysis at 50 °C for 24 h and discarding precipitate, followed by self-assembly at 50 °C for 24 h | Cai and Shi (2014) |
Potato | Pullulanase hydrolysis at 58 °C for 8 h and discarding precipitate, followed by self-assembly at 4 °C for 8 h | Jiang et al. (2016c) |
Pullulanase hydrolysis at 58 °C for 8 h and discarding precipitate, then addition of 0.1% of surfactant (SDS, Span 80 and Tween 80) based on solution, followed by self-assembly at 4 °C for 8 h | Li et al. (2016) | |
Proso millet | Pullulanase hydrolysis at 56 °C for 8 h and discarding precipitate, followed by self-assembly at 4 °C for 0.5, 4, 12 and 24 h |
Sun et al. (2014a) Gong et al. (2016) |
Maize | Pullulanase hydrolysis at 60 °C for 24 h and discarding precipitate, followed by self-assembly at 4 °C for 24 h | Luo et al. (2019b) |
Pullulanase hydrolysis at 56 °C for 8 h and discarding precipitate, followed by self-assembly at 4 °C for 12 h | Liu et al. (2016) | |
Chestnut | Pullulanase hydrolysis at 60 °C for 24 h and discarding precipitate, followed by self-assembly at 4 °C for 24 h | Luo et al. (2019b) |
Taro | Pullulanase hydrolysis at 58 °C for 8 h and discarding precipitate, then self-assembly at 4 °C for 8 h, followed by modification with octenyl succinic anhydride | Jiang et al. (2016a) |