. 2020 Apr 5;10(4):688. doi: 10.3390/nano10040688

Figure 10.

Figure 10

Effect of PDOP polymerization time (i.e., PDOP thickness) on SERS effect for 30 min of silver reduction time. Representative Raman measurements of the bimetallic core–shell NP system for different PDOP deposition times (numbers indicate deposition times in min). The final concentration of MB for Raman measurement is 10−5 M.