Skip to main content
. 2020 May 9;21(3):495–505. doi: 10.1007/s10561-020-09836-1

Table 2.

Mechanical properties of the poly lactic-co-glycolic acid (PLGA)/polyurethane (PU) (B) and poly-phosphate (poly-P) incorporated PLGA/PU nanofibrous scaffold (PLGA/PU/poly-P) obtained from tensile assay

Group Ultimate tensile strength (MPa) Elongation at break (%)
PLGA/PU 15.12 ± 2.16 32.13 ± 0.57
PLGA/PU/polyP 13.23 ± 1.25 39.45 ± 1.78