Table 4. CR at 30 °C of Different Electrodes in Both Anolyte and Catholyte.
electrodes | CR, gmd for the water chamber (catholyte) | CR, gmd in the MO chamber (anolyte) |
---|---|---|
Ni | 0 | 0.375 |
SS | 0.75 | 0.75 |
brass | 1.875 | 2.625 |