The effect of the initial protein concentration loaded on the physicochemical characteristics of the PLGA nanoparticles produced using microfluidics at FRR 1:1 and TFR 10 mL/min: a particle size (bars) and PDI (dots), b encapsulation efficiency (EE%) and c loading (wt/wt%) for PLGA 50:50, PLGA 75:25 and PLGA 85:15. Results represent mean ± SD of triplicate measurements