Fig. 1.

Fig. 1.

Indentation behavior and Vickers microhardness for ZIF-62 glass in the load range of 0.1 N to 1.96 N. (A) Indent images (note the different scale) for increasing load as shown by the arrow. (B) Microhardness (blue points) and crack initiation probability (red points) as a function of applied load. The dashed lines are guides for the eyes.