Skip to main content
. Author manuscript; available in PMC: 2021 Aug 1.
Published in final edited form as: Addit Manuf. 2020 Apr 23;34:101241. doi: 10.1016/j.addma.2020.101241

Table 2.

Hardness (H) and wear volume (V) for the four DED fabricated samples for values wear coefficient calculation. Normal load (W) was 5N and sliding distance (S) was 1000 m for all testing.

Ti64 5Si 10Si T32
Hardness (GPa) 3.86 6.20 8.29 7.87
Volume (m3) 1.61×10−9 1.33×10−9 4.68×10−10 7.87×10−10
Wear Coefficient (k) 1.24×10−6 1.65×10−6 7.76×10−7 1.07×10−6