Skip to main content
. 2020 Apr 18;12(4):373. doi: 10.3390/pharmaceutics12040373

Table 2.

Physical properties of the electrospinning solutions used to generate trilayered fibers.

Solution Concentration
(wt %)
Viscosity
(mPa·s)
Surface Tension
(mNm−1)
Conductivity
(µSm−1)
PCL + MTZ 12 + 4 1355.0 ± 6.4 40.2 ± 0.6 5.37 ± 0.04
PEG 25 1605.0 ± 5.0 39.0 ± 0.9 2.90 ± 0.02
PVP-I 10 4.1 ± 0.3 24.6 ± 0.3 340.00 ± 4.00
PVP + PVP-I
1:1 w/w
10 78.6 ± 1.2 27.8 ± 0.3 121.00 ± 0.50