Skip to main content
. Author manuscript; available in PMC: 2021 Apr 29.
Published in final edited form as: J Am Chem Soc. 2020 Apr 21;142(17):7783–7794. doi: 10.1021/jacs.9b13813

Table 1.

Physiochemical parameters for AcetalDextran-AuNP-Micelles and precursor gold nanoparticles.

% Au [w/w]a Core diameterb Hydrodynamic diameterc Solubilityd pH sensitivitye
pMBA-AuNPs 79.3% 1.7 ± 0.5 nm 5.0 nm
PDI: 0.251
Water No
Dextran-AuNPs 31.0% 2.1 ± 0.5 nm 7.3 nm
PDI: 0.246
Water, DMSO No
AcetalDextran-AuNPs 13.8% 2.1 ± 0.6 nm n/a Acetone, Toluene, Chloroform Yes
AcetalDextran-AuNP-Micelles 11.4% 111.1 ± 38 nm 146.0 nm
PDI: 0.156
Water Yes
a

Percent gold mass measured by ICP-OES.

b

Core diameters measured by transmission electron microscopy, expressed as the average of 40–100 particle measurements, ± standard deviation.

c

Hydrodynamic diameters measured by dynamic light scattering, expressed as the mean intensity and polydispersity index averaged for three measurements (pMBA-AuNPs and Dextran-AuNPs, one batch; AcetalDextran-AuNP-Micelles, six batches).

d

Solubility is not comprehensive.

e

pH sensitivity refers to observed changes in particle solubility and sedimentation behavior after incubation at pH 5.0.