. 2020 Mar 25;12(4):732. doi: 10.3390/polym12040732

Figure 4.

Figure 4

(a) Sample deflection recorded during creep tests for the sample PLA (squares), polyamide 11 (PA11) (diamond), PLA70 (circles), and PLA70-silicate at 3 wt.% (triangles). (b,c) The pictures show the samples PLA70 and PLA70-silicate at the end of the test, that is, after the temperature had reached ≈160 °C [38], Reproduced with permission from Nuzzo A, Macromol. Mater. Eng.; published by Wiley, 2014.