. 2020 Mar 25;12(4):732. doi: 10.3390/polym12040732

Figure 6.

Figure 6

(a) Elongation at break (EB) and (b) Young’s modulus (E) of different samples without and with montmorillonite and compatilizing agent as a function of accelerated weathering exposure, using UV-B lamps (~313 nm). (c) energy dispersive X-ray analysis (EDX) of Cloisite 15A [28], Reproduced with permission from Dintcheva NTz, Polym. Degrad. Stab.; published by Elsevier, 2009.