Residues of COT (A), COT+PA+BC(10) (B), COT+PA+BC(8) (C), COT+PA+BC(6) (D) and COT+PA+BC(4) (E) after cone calorimetry tests performed at 35 kW/m2. Residues of COT+PA+BC(10) (F), COT+PA+BC(8) (G) and COT+PA+BC(6) (H) after cone calorimetry tests performed at 50 kW/m2.