Skip to main content
. 2020 Apr 16;12(4):923. doi: 10.3390/polym12040923

Figure 9.

Figure 9

Surface resistivity measured at 30 °C (light blue) and 115 °C (light red) upon repeated cycles of the nanocomposite composed by PK30-Gly-Gly and lrGO. (A) 4 wt. %, (B) 5 wt. %, (C) 6 wt. %, (D) 7 wt. %, and (E) 8 wt. %. Sample thickness of 1.05 mm. (F) Asymptotic surface resistivity as average over last three thermal cycles.