Skip to main content
. 2020 Apr 16;12(4):923. doi: 10.3390/polym12040923

Figure 11.

Figure 11

Surface resistivity measured at 30 °C (light blue) and 115 °C (light red) upon repeated cycles of the nanocomposite composed by PK30-Gly-Gly and hrGO. 5 (A) and (B) 6 wt. % of filler. Sample thickness of 1.05 mm.