Skip to main content
. 2020 May 11;13(9):2200. doi: 10.3390/ma13092200

Table 1.

Processing parameters of composites.

P(3HB-co-4HB)/WF (Mass Ratio) Temperature of Plasticizing Zone (°C) Injection Temperature (°C) Injection Pressure (bar)
100 140 140 350
90/10 140 140 450
80/20 140 140 550
70/30 150 150 700
(100)/5 wt. % of nisin 140 140 350
(80/20)/5 wt. % of nisin 140 140 550