Skip to main content
. 2020 May 7;13(9):2156. doi: 10.3390/ma13092156

Figure 7.

Figure 7

Scanning electron microscope (SEM) images of polished surface of (a) 90:10, (b) 80:20, (c) 70:30, and (d) 60:40 wt % glass/Al2O3 composite samples.