Table 2.
Chirality quantification for RH and LH Au nanostructures formed after illumination with right-handed and left-handed CPL.
| LH Au NP | RH Au NP | |
|---|---|---|
| Osipov-Pickup-Dunmur Chirality Index (OPD) | 0.6493 | −4.965 |
| Hausdorff Chirality Measure (HCM) | 0.1343 | 0.1861 |
| Continuous Chirality Measure (CCM) | 1.315 | 1.738 |