Table 2.
Program | Ts | S | R 1 | T 1 | H 1 | R 2 | T 2 | H 2 | V 1 | V 2 | L | L t |
---|---|---|---|---|---|---|---|---|---|---|---|---|
Glazing VITABLOCS™ mark II | 600 | 4 | 70 | 950 | 1 | — | — | — | — | — | — | — |
| ||||||||||||
Crystallization and glazing IPS e.max® CAD | 403 | 6 | 90 | 820 | 10 | 30 | 840 | 7 | 550–820 | 820–840 | 700 | — |
| ||||||||||||
Metal oxidization IPS d.sign 10® | 403 | 4 | 80 | 950 | 1 | — | — | — | 450–950 | — | — | — |
| ||||||||||||
Firing and glazing IPS d.SIGN®, | ||||||||||||
Opaque | 403 | 6 | 80 | 890 | 1 | 450–889 | ||||||
Dentin | 403 | 6 | 60 | 870 | 1 | 450–869 | ||||||
Glazing | 403 | 4 | 60 | 870 | 1 | 450–869 |
T s: starting temperature (°C), R1: rate of firing stage 1 (°C/min), R2: rate of firing stage 2 (°C/min); (°C/min), T1: final temperature stage 1 (°C), T2: final temperature stage 2 (°C), S: prefiring, H1: holding time stage 1 (min), H2: holding time stage 2 (min), Lt: long term cooling, V1: vacuum starting temperature stage 1 (°C), V2: vacuum temperature stage 2, (°C).