Table 1. Comparison of the Performance of Various Hydrogen Peroxide Sensors.
electrode materials | linear range (μM) | detection limit (μM) | refs |
---|---|---|---|
MnO2 nanosheets | up to 454 | 0.005 | (63) |
graphene/Pt nanocomposite | 0.5–3475 | 0.2 | (64) |
Se/Pt nanocomposites | 10–15 000 | 3.1 | (65) |
RGO–Au–PTBO | 5.0–25 362 | 0.2 | (66) |
rGO@CeO2-AgNPs | 0.5–12 000 | 0.21 | (67) |
TiO2@Cu2O | 1–15 mM | 0.15 | (68) |
Au/GS/HRP/CS | 5–5130 | 1.7 | (69) |
cerium oxide NSs | 0.1–20 000 | 0.01 | this work |