(A,B) Crystallinity of PCL and ND-PCL composites and their representative differential scanning calorimetry (DSC) traces (n = 5). (C) Weight loss of samples in accelerated degradation experiments (n = 6). (D) Representative FTIR spectra of PCL and ND-PCL composites. (E) Inset showing FTIR spectra in the 400–1600 cm−1.