Composition of poly(epsilon caprolactone) (PCL) and poly(epsilon caprolactone)/poly(glycerol-sebacate)PCL/PGS polymeric solutions and parameters for electrospinning of PCL and PCL/PGS fiber mats.

Sample Name Label Solution Concentration [% w/v]/Polymer-BG Ratio PCL:PGS:BG Applied Voltage [kV] Distance Tip-Target [cm] Needle Diameter Flow Rate [mL/h] Temperature [oC] Relative Humidity [%]
PCL/PGSp S1 20/1:0.5:0 15 11 21G 0.4 24 ± 0.8 34 ± 12
PCL/PGSmxl S2 20/1:0.5:0 15 11 21G 0.4 24 ± 0.8 34 ± 12
PCL/PGSmxl/ 13-93 S3 20/1:0.5:0.3 15 11 18G 0.4 24 ± 0.8 34 ± 12
PCL/PGSmxl/ 13-93BS S4 20/1:0.5:0.3 15 11 18G 0.4 24 ± 0.8 34 ± 12
PCL S5 20/1:0:0 15 11 21G 0.4 24 ± 0.8 34 ± 12
PCL/13-93 S6 20/1:0:0.3 15 11 18G 0.4 24 ± 0.8 34 ± 12
PCL/13-93BS S7 20/1:0.5:0.3 15 11 18G 0.4 24 ± 0.8 34 ± 12