Skip to main content
. 2020 May 18;12(5):1153. doi: 10.3390/polym12051153

Figure 6.

Figure 6

(a) Elastic modulus and (b) flexural strength before (1) and after 4 weeks of the hydrothermal aging vs. carbon nanofiller’s (-s’) weight content heated at 70 °C (2) or immersed in water at 70 °C (3) (dots—experimental data, lines—polynomic approximations).