Thermal parameters for the thermograms of PWV with different loading of PF resin-filled OPA nanoparticles.

Type of Plywood Initial Degradation Temperature (°C) Maximum Degradation Temperature (°C) Residue (%)
PWV 0% 250 330 23
PWV 1% 255 339 24
PWV 2% 259 340. 25
PWV 3% 253 337 24
PWV 4% 254 338 26
PWV 5% 254 339 26