Table A2.
Characteristic quantities of PEO/PMMA blends with YS = 0.1 at 298 K
Y s | 1/0 | 0.75/0.25 | 0.5/0.5 | 0.25/0.75 |
---|---|---|---|---|
/s−1 | 8 × 104 | 1.35 × 105 | 9000 | 2.0 × 104 |
/s−1 | 4000 | 4000 | 200 | 1600 |
f+/s−1 | 1.5 × 106 | 1.0 × 106 | 4.1 × 104 | 1.1 × 105 |
n | 0.92 | 0.95 | 0.93 | 0.93 |
ε ∞ | 8.5 | 5.1 | 1.9 | 3.3 |
/s−1 | 3000 | 3000 | 150 | 1050 |
(tanδ)max | 5.8 | 10.0 | 12.9 | 4.7 |
d0.5/10−4 m | 1.42 | 1.55 | 2.0 | 1.55 |
λ/m | 1.3 × 10−6 | 3.5 × 10−7 | 2.8 × 10−7 | 1.5 × 10−6 |
σdc/A(V m)−1 | 5.6 × 10−5 | 5.1 × 10−5 | 2.1 × 10−6 | 5.4 × 10−6 |
fσ/s−1 | 6.3 × 105 | 3.6 × 105 | 4.0 × 104 | 5.9 × 104 |
DX/m2 s−1 | 9.9 × 10−14 | 1.25 × 10−14 | 4.8 × 10−16 | 1.5 × 10−15 |
c/c0 | 1.2 × 10−7 | 7.3 × 10−7 | 6.5 × 10−7 | 3.1 × 10−8 |
vdrift/m s−1 | 4.0 | 0.30 | 0.016 | 0.19 |